A UHV surface analysis system for thin film depth profiling

Hiden Analytical provides extremely versatile high-sensitivity instrumentation for high performance dynamic and static SIMS (secondary ion mass spectrometry) analysis, unlocking new levels of precision in cutting-edge applications. With an extended range and the ability to acquire and identify both positive (+ve) and negative (-ve) secondary ions, the SIMS workstation is a comprehensive solution for composition analysis and depth profiling applications.

For simultaneous +ve and -ve ion analysis in a comprehensive SIMS package, Hiden Analytical has also developed the innovative Hi5 SIMS workstation. Find more information in our product literature below.

Overview

Secondary ion mass spectrometry, or SIMS, is one of the most sensitive techniques ever developed for interrogating the uppermost surface layers of a material, from depths of several hundred nanometres (nm) to a single atomic layer. It can obtain compositional data down to the parts per billion (ppb) range and is compatible with any material that can reliably be tested in vacuum conditions. Consequently, SIMS instruments are routinely used to analyse ceramics, metals, organic materials, polymers, semiconductors, and more.

This technique is broken down into two distinct methodologies: dynamic and static SIMS. Each of these uses a primary ion beam that impacts a sample in vacuum conditions, causing extremely small volumes of material to be ablated from the surface – a fraction of this ejected material will be ionised. These secondary ions are acquired by the sample inlet of the mass spectrometry unit to develop a robust understanding of the composition of the specimen’s uppermost surface layers.

The primary difference between dynamic and static SIMS is the ion dosage (a higher dose for dynamic SIMS instruments), and that dynamic SIMS cannot be run with a defocussed ion beam; it must be raster scanned across the sample surface to produce a flat-bottomed crater. Hiden Analytical’s SIMS workstation can perform both dynamic and static SIMS analysis in a single consolidated SIMS instrument. With a dual-mode MAXIM mass spectrometer, the SIMS workstation can operate in secondary ion detection mode for +ve/-ve ion detection, and in a secondary neutral detection mode for +ve data quantification. Each mode is compatible with mass range options up to 5000 atomic mass units (amu).

Hiden Analytical’s SIMS Workstation

Our SIMS workstation is a comprehensive solution for depth profiling and compositional analysis of samples in various areas of surface analysis, thin film engineering, nanotechnology, fuel cell research, and more. The system is highly customizable to suit the unique requirements of users in complex fields.

How to Analyse the Top Nano Layers of a Material

If you need more information about performing static or dynamic SIMS analysis, browse our product literature and presentations. For a more detailed insight into the features of our SIMS workstation, simply contact a member of the Hiden Analytical team today.

Features

Related Products

Further Reading

The SIMS Mapper software provides a simple, but powerful, user interface to the SIMS tool.  The species to be analysed are chosen from a period table view, with mass interferences highlighted, and the data are collected as images throughout the analysis.  For depth profiles the gated area can be defined after analysis and images may be stacked to reconstruct the concentration profile in three dimensions.  For less experienced operators, or in a production environment, analyses can be run from previously stored templates and fully automated “queued” running is possible with the automatic stage option.  A range of data export formats allows results to be used by other software packages for enhanced display or processing.

  • 3D imaging
  • depth profiling with highly flexible gating
  • simple choice of species
  • easy set-up for inexperienced users yet full control for experts
  • large live interactive image and depth profile windows
  • export in .csv and proprietary formats
Icon

Optimisation of the connection between TA-MS systems together with improved data interpretation for TA-MS applications. 1.98 MB 74 downloads

Optimisation of the connection between TA-MS systems together with improved data...
Icon

High-temperature oxidation of CrN/AlN multilayer coatings. 605.40 KB 70 downloads

High-temperature oxidation of CrN/AlN multilayer coatings. ...
Icon

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. 1.94 MB 67 downloads

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. ...
Icon

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer water. 2.35 MB 71 downloads

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer...
Icon

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. 207.58 KB 72 downloads

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. ...
Icon

End point detection in ion beam milling of YB2 Cu3 07 thin films. 4.15 MB 67 downloads

End point detection in ion beam milling of YB2 Cu3 07 thin films. ...
Icon

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and indium. 252.94 KB 67 downloads

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and...
Icon

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. 1.36 MB 67 downloads

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. ...
Icon

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour deposition system. 1.03 MB 71 downloads

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour...