For the determination of surface composition, contaminant analysis and depth profiling

SIMS is a high sensitivity surface analysis technique for the determination of surface composition, contaminant analysis and for depth profiling in the uppermost surface layers of a sample.

Overview

SIMS is a high sensitivity surface analysis technique for the determination of surface composition, contaminant analysis and for depth profiling in the uppermost surface layers of a sample.

Applied to analysis within the first few microns of a surface, Hiden’s SIMS systems provide depth profiles with depth resolution to 2 nanometres.

The Hiden SIMS Workstation provides for high performance static and dynamic SIMS applications for detailed surface composition analysis and depth profiling.

Hiden’s elemental SIMS imaging facility provides for high resolution surface chemical mapping.

Hiden Bolt-On Components are available for upgrading existing surface analysis equipment with SIMS facilities.

Further Reading

Icon

MXene improves the stability and electrochemical performance of electropolymerized PEDOT films 6.69 MB 0 downloads

MXene improves the stability and electrochemical performance of electropolymerized...
Icon

Growth of conductive Si-doped α-Ga2O3 by suboxide molecular-beam epitaxy 5.68 MB 0 downloads

Growth of conductive Si-doped α-Ga2O3 by suboxide molecular-beam epitaxy ...
Icon

Impact of oxygen and hydrogen traces on the focused ion beam sputter rate and secondary ion mass spectrometry intensity detection of graphite 2.66 MB 3 downloads

Impact of oxygen and hydrogen traces on the focused ion beam sputter rate and secondary...
Icon

On the knowledge of depth effect on secondary ion mass spectrometry profiling of deuterium-implanted fusion matrices 4.51 MB 12 downloads

On the knowledge of depth effect on secondary ion mass spectrometry profiling of...
Icon

On the knowledge of depth effect on secondary ion mass spectrometry profiling of deuterium-implanted fusion matrices 4.51 MB 14 downloads

On the knowledge of depth effect on secondary ion mass spectrometry profiling of...
Icon

Probing dynamic degradation and mass transport in solid-state sodium-ion batteries using operando simultaneous dual-polarity SIMS 3.42 MB 14 downloads

Probing dynamic degradation and mass transport in solid-state sodium-ion batteries...
Icon

Application of Secondary Ion Mass Spectrometry for Analysis of Decorative Coatings on Fancy Goods Accessories 1.33 MB 106 downloads

Application of Secondary Ion Mass Spectrometry for Analysis of Decorative Coatings...
Icon

Alkali-metal-based molecular-ion secondary ion mass spectrometry for precise quantitative analysis of low-dimensional materials without standards 3.01 MB 98 downloads

Alkali-metal-based molecular-ion secondary ion mass spectrometry for precise quantitative...
Icon

The crucial role of defect structure in understanding the electrical properties of spark plasma sintered antimony doped barium stannate 1.74 MB 124 downloads

The crucial role of defect structure in understanding the electrical properties of...
Icon

Silicon-doped β-Ga2O3 films grown at 1 μm/h by suboxide molecular-beam epitaxy 1.33 MB 137 downloads

Silicon-doped β-Ga2O3 films grown at 1 μm/h by suboxide molecular-beam epitaxy ...