SIMS Workstation

For further information and pricing, please get in touch with us.

A UHV surface analysis system for thin film depth profiling

Hiden Analytical provides extremely versatile high-sensitivity instrumentation for high performance dynamic and static SIMS (secondary ion mass spectrometry) analysis, unlocking new levels of precision in cutting-edge applications. With an extended range and the ability to acquire and identify both positive (+ve) and negative (-ve) secondary ions, the SIMS workstation is a comprehensive solution for composition analysis and depth profiling applications.

For simultaneous +ve and -ve ion analysis in a comprehensive SIMS package, Hiden Analytical has also developed the innovative Hi5 SIMS workstation. Find more information in our product literature below.

Overview

Secondary ion mass spectrometry, or SIMS, is one of the most sensitive techniques ever developed for interrogating the uppermost surface layers of a material, from depths of several hundred nanometres (nm) to a single atomic layer. It can obtain compositional data down to the parts per billion (ppb) range and is compatible with any material that can reliably be tested in vacuum conditions. Consequently, SIMS instruments are routinely used to analyse ceramics, metals, organic materials, polymers, semiconductors, and more.

This technique is broken down into two distinct methodologies: dynamic and static SIMS. Each of these uses a primary ion beam that impacts a sample in vacuum conditions, causing extremely small volumes of material to be ablated from the surface – a fraction of this ejected material will be ionised. These secondary ions are acquired by the sample inlet of the mass spectrometry unit to develop a robust understanding of the composition of the specimen’s uppermost surface layers.

The primary difference between dynamic and static SIMS is the ion dosage (a higher dose for dynamic SIMS instruments), and that dynamic SIMS cannot be run with a defocussed ion beam; it must be raster scanned across the sample surface to produce a flat-bottomed crater. Hiden Analytical’s SIMS workstation can perform both dynamic and static SIMS analysis in a single consolidated SIMS instrument. With a dual-mode MAXIM mass spectrometer, the SIMS workstation can operate in secondary ion detection mode for +ve/-ve ion detection, and in a secondary neutral detection mode for +ve data quantification. Each mode is compatible with mass range options up to 5000 atomic mass units (amu).

Hiden Analytical’s SIMS Workstation

Our SIMS workstation is a comprehensive solution for depth profiling and compositional analysis of samples in various areas of surface analysis, thin film engineering, nanotechnology, fuel cell research, and more. The system is highly customizable to suit the unique requirements of users in complex fields.

How to Analyse the Top Nano Layers of a Material

If you need more information about performing static or dynamic SIMS analysis, browse our product literature and presentations. For a more detailed insight into the features of our SIMS workstation, simply contact a member of the Hiden Analytical team today.

Features

Related Products

Further Reading

The SIMS Mapper software provides a simple, but powerful, user interface to the SIMS tool.  The species to be analysed are chosen from a period table view, with mass interferences highlighted, and the data are collected as images throughout the analysis.  For depth profiles the gated area can be defined after analysis and images may be stacked to reconstruct the concentration profile in three dimensions.  For less experienced operators, or in a production environment, analyses can be run from previously stored templates and fully automated “queued” running is possible with the automatic stage option.  A range of data export formats allows results to be used by other software packages for enhanced display or processing.

  • 3D imaging
  • depth profiling with highly flexible gating
  • simple choice of species
  • easy set-up for inexperienced users yet full control for experts
  • large live interactive image and depth profile windows
  • export in .csv and proprietary formats
Icon

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy and secondary ion mass spectrometry 48.00 KB 0 downloads

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 48.00 KB 0 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged ions in sputtering process 48.00 KB 0 downloads

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged...
Icon

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of (Zn1-zInz)(O1-xNx) Solid Solution 48.00 KB 0 downloads

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of...
Icon

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics of chemically synthesized ZnO nanowalls 48.00 KB 0 downloads

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics...
Icon

Modified photoluminescence and photodetection characteristics of chemically grown SnO coated ZnO nanoneedles 48.00 KB 0 downloads

Modified photoluminescence and photodetection characteristics of chemically grown...
Icon

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials without standards 48.00 KB 0 downloads

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials...
Icon

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions 48.00 KB 0 downloads

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions ...
Icon

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO 48.00 KB 0 downloads

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO ...
Icon

Towards an Understanding of MCs+n Formation Mechanism in SIMS 1.94 MB 92 downloads

Towards an understanding of MCs+n formation mechanism in SIMS. ...