SNMS of Magnetic Storage Materials

For further information and pricing, please get in touch with us.

Depth profiling and quantified composition of alloys using SNMS.

SNMS provides excellent depth resolution and quantification to analyse the layer structure of the hard disc head material and the active region of the platter surface itself.

Overview

SNMS provides excellent depth resolution and quantification to analyse the layer structure of the hard disc head material (top) and the active region of the platter surface itself (bottom).

Sputtered Neutral Mass Spectrometry

Sputtered Neutral mass Spectrometry separates the ionisation event from the sputtering and thus overcomes the matrix effect which makes high concentration quantification difficult in conventional SIMS analysis.

The MAXIM spectrometer uses a high efficiency electron impact ioniser to detect the sputtered neutral flux after secondary ions have been removed by means of an external deflector.

With no significant matrix effect there is no need for matrix matched reference materials, as is the case with SIMS, and easily available alloys may be used to determine global sensitivity factors.

Oxygen Flood

Low energy beams give improved depth resolution but can also induce surface topography. A directional jet of pure oxygen is provided over the
sample surface, fully oxidising the surface via a stainless steel capillary.

The gives enhancements in sensitivity for the analysis of electropositive species such as metals and semiconductor dopants, as well as reductions in surface roughness in low beam energy, high depth resolution analyses.

The examples show the improvements in surface topography given by the use of the localised oxygen flood in a 3.6 nm multilayer Si/Fe sample.

Without oxygen flood depth resolution decays (Left). With oxygen flood depth resolution is maintained (Right).

Further Reading

Icon

Interaction of molecular oxygen ions with copper surface: features of the energy spectra of sputtered and backscattered ions 511.39 KB 138 downloads

Interaction of molecular oxygen ions with copper surface: features of the energy...
Icon

P-type conductivity in Sn-doped Sb2 Se3 2.64 MB 134 downloads

P-type conductivity in Sn-doped Sb2 Se3 ...
Icon

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives for Li-Ion Batteries 3.75 MB 171 downloads

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives...
Icon

Robust nonfullerene solar cells approaching unity external quantum efficiency enabled by suppression of geminate recombination 1.05 MB 138 downloads

Robust nonfullerene solar cells approaching unity external quantum efficiency...
Icon

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz Oxide by Interfacial Atomic Surface Reduction 4.22 MB 135 downloads

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 1,011.83 KB 130 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS 1.03 MB 81 downloads

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS ...
Icon

Large area visualization of the Li distribution in lithium-ion battery electrodes using plasma FIB and SIMS 384.40 KB 73 downloads

Large area visualization of the Li distribution in lithium-ion battery electrodes...
Icon

Low-frequency plasma activation of nylon 6 - Download 2.63 MB 71 downloads

Low-frequency plasma activation of nylon 6 ...
Icon

Wafer-level uniformity of atomic-layer-deposited niobium nitride thin films for quantum devices 1.92 MB 60 downloads

Wafer-level uniformity of atomic-layer-deposited niobium nitride thin films for...