SNMS of Magnetic Storage Materials

For further information and pricing, please get in touch with us.

Depth profiling and quantified composition of alloys using SNMS.

SNMS provides excellent depth resolution and quantification to analyse the layer structure of the hard disc head material and the active region of the platter surface itself.

Overview

SNMS provides excellent depth resolution and quantification to analyse the layer structure of the hard disc head material (top) and the active region of the platter surface itself (bottom).

Sputtered Neutral Mass Spectrometry

Sputtered Neutral mass Spectrometry separates the ionisation event from the sputtering and thus overcomes the matrix effect which makes high concentration quantification difficult in conventional SIMS analysis.

The MAXIM spectrometer uses a high efficiency electron impact ioniser to detect the sputtered neutral flux after secondary ions have been removed by means of an external deflector.

With no significant matrix effect there is no need for matrix matched reference materials, as is the case with SIMS, and easily available alloys may be used to determine global sensitivity factors.

Oxygen Flood

Low energy beams give improved depth resolution but can also induce surface topography. A directional jet of pure oxygen is provided over the
sample surface, fully oxidising the surface via a stainless steel capillary.

The gives enhancements in sensitivity for the analysis of electropositive species such as metals and semiconductor dopants, as well as reductions in surface roughness in low beam energy, high depth resolution analyses.

The examples show the improvements in surface topography given by the use of the localised oxygen flood in a 3.6 nm multilayer Si/Fe sample.

Without oxygen flood depth resolution decays (Left). With oxygen flood depth resolution is maintained (Right).

Further Reading

Icon

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization... 330.25 KB 72 downloads

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization...
Icon

Surface Analysis by Secondary-Ion Mass Spectroscopy During Etching with Gas-Cluster Ion Beam 153.58 KB 85 downloads

Surface analysis by secondary-ion mass spectroscopy during etching with gas-cluster...
Icon

Sputter Depth Profiling by Secondary Ion Mass Spectrometry Coupled with Sample Current... 613.21 KB 78 downloads

Sputter depth profiling by secondary ion mass spectrometry coupled with sample current...
Icon

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS and... 109.76 KB 76 downloads

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS...
Icon

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective 1.94 MB 76 downloads

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective. ...
Icon

Plasma Implanted Ultra Shallow Junction Boron Depth Profiles: Effect of Plasma Chemistry... 618.05 KB 79 downloads

Plasma implanted ultra shallow junction boron depth profiles: Effect of plasma chemistry...
Icon

Mass-Resolved Ion Scattering Spectrometry for Characterization of Samples with Historical... 200.29 KB 74 downloads

Mass-resolved ion scattering spectrometry for characterization of samples with historical...
Icon

Interfacial Diffusion in a Double Quantum Well Structure 1.94 MB 86 downloads

Interfacial diffusion in a double quantum well structure. ...
Icon

Interface-Dominated Growth of a Metastable Novel Alloy Phase 1.94 MB 74 downloads

Interface-dominated Growth of a Metastable Novel Alloy Phase. ...
Icon

Instantaneous Surface Work Function Dependence of MCs+n Molecular Ion Emission Under... 1.94 MB 71 downloads

Instantaneous surface work function dependence of MCs+n molecular ion emission under...