Depth profile through a Copper Indium Gallium Selenide (CIGS) solar cell showing high dynamic range and good depth resolution.

The depth scale is left as analytical cycles, showing that high data density can be achieved even when a large number of elements are detected. The overall depth is around 4 microns.

Overview

Depth profile through a Copper Indium Gallium Selenide (CIGS) solar cell showing high dynamic range and good depth resolution.

The depth scale is left as analytical cycles, showing that high data density can be achieved even when a large number of elements are detected. The overall depth is around 4 microns.

Zinc in GaAs

Using caesium primary ions, the species of interest is measured as a molecule together with a Cs+ ion. For some elements, such as Zn, the ion ZnCs+ is actually more sensitive than detecting either Zn+ or Zn– ions.

Further Reading

Icon

Interaction of molecular oxygen ions with copper surface: features of the energy spectra of sputtered and backscattered ions 511.39 KB 138 downloads

Interaction of molecular oxygen ions with copper surface: features of the energy...
Icon

P-type conductivity in Sn-doped Sb2 Se3 2.64 MB 134 downloads

P-type conductivity in Sn-doped Sb2 Se3 ...
Icon

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives for Li-Ion Batteries 3.75 MB 171 downloads

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives...
Icon

Robust nonfullerene solar cells approaching unity external quantum efficiency enabled by suppression of geminate recombination 1.05 MB 138 downloads

Robust nonfullerene solar cells approaching unity external quantum efficiency...
Icon

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz Oxide by Interfacial Atomic Surface Reduction 4.22 MB 135 downloads

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 1,011.83 KB 130 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS 1.03 MB 81 downloads

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS ...
Icon

Large area visualization of the Li distribution in lithium-ion battery electrodes using plasma FIB and SIMS 384.40 KB 73 downloads

Large area visualization of the Li distribution in lithium-ion battery electrodes...
Icon

Low-frequency plasma activation of nylon 6 - Download 2.63 MB 71 downloads

Low-frequency plasma activation of nylon 6 ...
Icon

Wafer-level uniformity of atomic-layer-deposited niobium nitride thin films for quantum devices 1.92 MB 60 downloads

Wafer-level uniformity of atomic-layer-deposited niobium nitride thin films for...