Depth profile through a Copper Indium Gallium Selenide (CIGS) solar cell showing high dynamic range and good depth resolution.

The depth scale is left as analytical cycles, showing that high data density can be achieved even when a large number of elements are detected. The overall depth is around 4 microns.

Overview

Depth profile through a Copper Indium Gallium Selenide (CIGS) solar cell showing high dynamic range and good depth resolution.

The depth scale is left as analytical cycles, showing that high data density can be achieved even when a large number of elements are detected. The overall depth is around 4 microns.

Zinc in GaAs

Using caesium primary ions, the species of interest is measured as a molecule together with a Cs+ ion. For some elements, such as Zn, the ion ZnCs+ is actually more sensitive than detecting either Zn+ or Zn– ions.

Further Reading

Icon

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy and secondary ion mass spectrometry 48.00 KB 0 downloads

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 48.00 KB 0 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged ions in sputtering process 48.00 KB 0 downloads

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged...
Icon

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of (Zn1-zInz)(O1-xNx) Solid Solution 48.00 KB 0 downloads

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of...
Icon

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics of chemically synthesized ZnO nanowalls 48.00 KB 0 downloads

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics...
Icon

Modified photoluminescence and photodetection characteristics of chemically grown SnO coated ZnO nanoneedles 48.00 KB 0 downloads

Modified photoluminescence and photodetection characteristics of chemically grown...
Icon

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials without standards 48.00 KB 0 downloads

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials...
Icon

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions 48.00 KB 0 downloads

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions ...
Icon

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO 48.00 KB 0 downloads

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO ...
Icon

Towards an Understanding of MCs+n Formation Mechanism in SIMS 1.94 MB 92 downloads

Towards an understanding of MCs+n formation mechanism in SIMS. ...