Ion implantation and diffusion is used to deliver dopants into semiconductors, SIMS accurately measures the dopant concentration for process development and monitoring.

The examples below show quantified depth profiles in silicon substrates

Overview

Ion implantation and diffusion is used to deliver dopants into semiconductors, SIMS accurately measures the dopant
concentration for process development and monitoring.

The examples below show quantified depth profiles in silicon substrates.

Further Reading

Icon

Interaction of molecular oxygen ions with copper surface: features of the energy spectra of sputtered and backscattered ions 511.39 KB 138 downloads

Interaction of molecular oxygen ions with copper surface: features of the energy...
Icon

P-type conductivity in Sn-doped Sb2 Se3 2.64 MB 134 downloads

P-type conductivity in Sn-doped Sb2 Se3 ...
Icon

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives for Li-Ion Batteries 3.75 MB 171 downloads

Controlling Li Dendritic Growth in Graphite Anodes by Potassium Electrolyte Additives...
Icon

Robust nonfullerene solar cells approaching unity external quantum efficiency enabled by suppression of geminate recombination 1.05 MB 138 downloads

Robust nonfullerene solar cells approaching unity external quantum efficiency...
Icon

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz Oxide by Interfacial Atomic Surface Reduction 4.22 MB 135 downloads

Mitigating Structural Instability of High-Energy Lithium- and Manganese-Rich LiNixMnyCoz...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 1,011.83 KB 130 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS 1.03 MB 81 downloads

Analysis of useful ion yield for the Mg dopant in GaN by quadrupole—SIMS ...
Icon

Large area visualization of the Li distribution in lithium-ion battery electrodes using plasma FIB and SIMS 384.40 KB 73 downloads

Large area visualization of the Li distribution in lithium-ion battery electrodes...
Icon

Low-frequency plasma activation of nylon 6 - Download 2.63 MB 71 downloads

Low-frequency plasma activation of nylon 6 ...
Icon

Wafer-level uniformity of atomic-layer-deposited niobium nitride thin films for quantum devices 1.92 MB 60 downloads