Select Page

Electronic materials

For further information and pricing, please get in touch with us.

Ion implantation and diffusion is used to deliver dopants into semiconductors, SIMS accurately measures the dopant concentration for process development and monitoring.

The examples below show quantified depth profiles in silicon substrates

Overview

Ion implantation and diffusion is used to deliver dopants into semiconductors, SIMS accurately measures the dopant
concentration for process development and monitoring.

The examples below show quantified depth profiles in silicon substrates.

Further Reading

Icon

Optimisation of the connection between TA-MS systems together with improved data interpretation for TA-MS applications. 1.98 MB 74 downloads

Optimisation of the connection between TA-MS systems together with improved data...
Icon

High-temperature oxidation of CrN/AlN multilayer coatings. 605.40 KB 70 downloads

High-temperature oxidation of CrN/AlN multilayer coatings. ...
Icon

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. 1.94 MB 67 downloads

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. ...
Icon

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer water. 2.35 MB 71 downloads

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer...
Icon

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. 207.58 KB 72 downloads

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. ...
Icon

End point detection in ion beam milling of YB2 Cu3 07 thin films. 4.15 MB 67 downloads

End point detection in ion beam milling of YB2 Cu3 07 thin films. ...
Icon

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and indium. 252.94 KB 67 downloads

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and...
Icon

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. 1.36 MB 67 downloads

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. ...
Icon

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour deposition system. 1.03 MB 71 downloads

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour...