Select Page

Contamination

Contamination_320x200px_shutterstock_550112053
For further information and pricing, please get in touch with us.

Imaging and mass spectra to locate and identify surface contamination.

Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

Overview

Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

contamination on diesel injector component

The mass resolved image shows the distribution of 56Fe. The inset identifies the region where the stain was observed; as the Fe signal is masked by the surface contaminant.

A mass spectrum taken on the clean base surface shows the composition to be mainly Fe and Cr (with some Na from handling). A similar spectrum from the stain is dominated by the 40Ca signal with the metal signals being significantly reduced.

The stain is positively identified as being Ca based and originating from use of bio-diesel. This known possible fuel contaminant is limited by EU regulations to 5 mg/kg (summed with the Mg content).

Diesel injector

Further Reading

Icon

Optimisation of the connection between TA-MS systems together with improved data interpretation for TA-MS applications. 1.98 MB 74 downloads

Optimisation of the connection between TA-MS systems together with improved data...
Icon

High-temperature oxidation of CrN/AlN multilayer coatings. 605.40 KB 70 downloads

High-temperature oxidation of CrN/AlN multilayer coatings. ...
Icon

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. 1.94 MB 67 downloads

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. ...
Icon

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer water. 2.35 MB 71 downloads

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer...
Icon

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. 207.58 KB 72 downloads

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. ...
Icon

End point detection in ion beam milling of YB2 Cu3 07 thin films. 4.15 MB 67 downloads

End point detection in ion beam milling of YB2 Cu3 07 thin films. ...
Icon

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and indium. 252.94 KB 67 downloads

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and...
Icon

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. 1.36 MB 67 downloads

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. ...