Imaging and mass spectra to locate and identify surface contamination.

Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

Overview

Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

contamination on diesel injector component

The mass resolved image shows the distribution of 56Fe. The inset identifies the region where the stain was observed; as the Fe signal is masked by the surface contaminant.

A mass spectrum taken on the clean base surface shows the composition to be mainly Fe and Cr (with some Na from handling). A similar spectrum from the stain is dominated by the 40Ca signal with the metal signals being significantly reduced.

The stain is positively identified as being Ca based and originating from use of bio-diesel. This known possible fuel contaminant is limited by EU regulations to 5 mg/kg (summed with the Mg content).

Diesel injector

Further Reading

Icon

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy and secondary ion mass spectrometry 48.00 KB 0 downloads

ZnS nanoparticle decorated ZnO nanowall network: investigation through electron microscopy...
Icon

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) 48.00 KB 0 downloads

Towards x-ray waveguide formation upon ion irradiation of a Co thin film on Si(111) ...
Icon

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged ions in sputtering process 48.00 KB 0 downloads

Symmetric and asymmetric collision effects on the formation of singly and doubly-charged...
Icon

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of (Zn1-zInz)(O1-xNx) Solid Solution 48.00 KB 0 downloads

Structure, Electronic Structure, Optical, and Dehydrogenation Catalytic Study of...
Icon

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics of chemically synthesized ZnO nanowalls 48.00 KB 0 downloads

Secondary ion mass spectrometry and photoluminescence study on microstructural characteristics...
Icon

Modified photoluminescence and photodetection characteristics of chemically grown SnO coated ZnO nanoneedles 48.00 KB 0 downloads

Modified photoluminescence and photodetection characteristics of chemically grown...
Icon

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials without standards 48.00 KB 0 downloads

MCsn +-SIMS: an innovative approach for direct compositional analysis of materials...
Icon

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions 48.00 KB 0 downloads

Inelastic ion-surface collisions: Understanding secondary emission of molecular ions ...
Icon

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO 48.00 KB 0 downloads

Electronic Structure and Catalytic Study of Solid Solutions of GaN in ZnO ...
Icon

Towards an Understanding of MCs+n Formation Mechanism in SIMS 1.94 MB 92 downloads

Towards an understanding of MCs+n formation mechanism in SIMS. ...