Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

Overview

Visible staining was observed on internal angled face of a diesel engine injector component. The stain was too thin to be detected by EDX.

contamination on diesel injector component

The mass resolved image shows the distribution of 56Fe. The inset identifies the region where the stain was observed; as the Fe signal is masked by the surface contaminant.

A mass spectrum taken on the clean base surface shows the composition to be mainly Fe and Cr (with some Na from handling). A similar spectrum from the stain is dominated by the 40Ca signal with the metal signals being significantly reduced.

The stain is positively identified as being Ca based and originating from use of bio-diesel. This known possible fuel contaminant is limited by EU regulations to 5 mg/kg (summed with the Mg content).

Diesel injector

Further Reading

Icon

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization... 330.25 KB 72 downloads

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization...
Icon

Surface Analysis by Secondary-Ion Mass Spectroscopy During Etching with Gas-Cluster Ion Beam 153.58 KB 85 downloads

Surface analysis by secondary-ion mass spectroscopy during etching with gas-cluster...
Icon

Sputter Depth Profiling by Secondary Ion Mass Spectrometry Coupled with Sample Current... 613.21 KB 78 downloads

Sputter depth profiling by secondary ion mass spectrometry coupled with sample current...
Icon

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS and... 109.76 KB 76 downloads

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS...
Icon

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective 1.94 MB 76 downloads

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective. ...
Icon

Plasma Implanted Ultra Shallow Junction Boron Depth Profiles: Effect of Plasma Chemistry... 618.05 KB 79 downloads

Plasma implanted ultra shallow junction boron depth profiles: Effect of plasma chemistry...
Icon

Mass-Resolved Ion Scattering Spectrometry for Characterization of Samples with Historical... 200.29 KB 74 downloads

Mass-resolved ion scattering spectrometry for characterization of samples with historical...
Icon

Interfacial Diffusion in a Double Quantum Well Structure 1.94 MB 86 downloads

Interfacial diffusion in a double quantum well structure. ...
Icon

Interface-Dominated Growth of a Metastable Novel Alloy Phase 1.94 MB 74 downloads

Interface-dominated Growth of a Metastable Novel Alloy Phase. ...
Icon

Instantaneous Surface Work Function Dependence of MCs+n Molecular Ion Emission Under... 1.94 MB 71 downloads

Instantaneous surface work function dependence of MCs+n molecular ion emission under...