Select Page

Pharmaceuticals

For further information and pricing, please get in touch with us.

Identification of molecular signals using static SIMS on powders

SIMS can be used to confirm the presence of a drug or to make brand identification where different formulations exist

Overview

SIMS can be used to confirm the presence of a drug or to make brand identification where different formulations exist; a branded product may contain additional substances or a counterfeit product could show contamination.

The presence of binding, dehydrating or filling agents can also provide a unique fingerprint. In the example below, Al and Na come from the pill forming material. The high sensitivity of the analyser allows very low beam currents to be employed, keeping below the static SIMS limit preserves the high mass fragments required for unequivocal identification.

Powder Analysis

Powders may be analysed using SIMS, both for bulk composition and core-shell structure. Powders can be mounted using either conductive adhesive tape, dispersion, pill formation or pressing into indium sheet.

Further Reading

Icon

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization... 330.25 KB 72 downloads

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization...
Icon

Surface Analysis by Secondary-Ion Mass Spectroscopy During Etching with Gas-Cluster Ion Beam 153.58 KB 85 downloads

Surface analysis by secondary-ion mass spectroscopy during etching with gas-cluster...
Icon

Sputter Depth Profiling by Secondary Ion Mass Spectrometry Coupled with Sample Current... 613.21 KB 78 downloads

Sputter depth profiling by secondary ion mass spectrometry coupled with sample current...
Icon

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS and... 109.76 KB 76 downloads

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS...
Icon

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective 1.94 MB 76 downloads

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective. ...
Icon

Plasma Implanted Ultra Shallow Junction Boron Depth Profiles: Effect of Plasma Chemistry... 618.05 KB 79 downloads

Plasma implanted ultra shallow junction boron depth profiles: Effect of plasma chemistry...
Icon

Mass-Resolved Ion Scattering Spectrometry for Characterization of Samples with Historical... 200.29 KB 74 downloads

Mass-resolved ion scattering spectrometry for characterization of samples with historical...
Icon

Interfacial Diffusion in a Double Quantum Well Structure 1.94 MB 86 downloads

Interfacial diffusion in a double quantum well structure. ...
Icon

Interface-Dominated Growth of a Metastable Novel Alloy Phase 1.94 MB 74 downloads

Interface-dominated Growth of a Metastable Novel Alloy Phase. ...
Icon

Instantaneous Surface Work Function Dependence of MCs+n Molecular Ion Emission Under... 1.94 MB 71 downloads

Instantaneous surface work function dependence of MCs+n molecular ion emission under...