Select Page

Surgical Stent

For further information and pricing, please get in touch with us.

Stents are wireframe scaffolds, used to hold narrowed arteries open.

Surface condition of the stent is very important and SIMS can be used to examine the nanometre thick protective chromium dioxide layer which naturally forms on the material.

Overview

Stents are wireframe scaffolds, typically laser cut from stainless steel, use to hold narrowed arteries open. Inserted via a catheter, the mesh is placed in the narrow area and expanded using a small balloon which is then withdrawn.

Surface condition of the stent is very important, and SIMS can be used to examine the nanometre thick protective chromium dioxide layer which naturally forms on the material. The depth profiles below show how treating with a chlorine-based disinfecting product leaves the surface iron rich and open to corrosion, potentially causing failure or tissue damage.

Limit of Detection

SIMS is the surface analysis technique with the best limit of detection (LOD), often providing ppm and even ppb measurement. If no interfering signals are present, the actual limit of detection depends on the ionisation probability of the sought species, the transmission of the instrument and the analyte volume. Thus, as first two parameters are fixed, if the volume is very small, there will be insufficient atoms present for detection. By collecting the data as images, the pixel sizes can be summed laterally or over a number of cycles to effectively increase the analyte volume and improve the LOD. This means that lateral and depth resolutions can be mutually traded to optimise an analysis for the most desirable parameter.

Ion Beam Polarity and Chemistry

The secondary ions emitted from the specimen usually have a favoured polarity. For instance, alkali metals are emitted as positive ions and halogens as negative. The probability of ion formation is also enhanced by using oxygen for electropositive elements and caesium for electronegative elements. In addition, caesium can be used in the CsM+ mode, where the element of interest, M, is detected as a molecule with Cs. The CsM+ mode is an excellent means of detecting and quantifying metal oxides and other materials where both electropositive and electronegative elements are sought.

Stents may be coated with polymer layers for protection or to elute drugs into the region to prevent future blockage. Static SIMS can detect and characterise this layer.

Negative secondary ion image of the coated stent displays a very unifrom polymer layer

Further Reading

Icon

Optimisation of the connection between TA-MS systems together with improved data interpretation for TA-MS applications. 1.98 MB 74 downloads

Optimisation of the connection between TA-MS systems together with improved data...
Icon

High-temperature oxidation of CrN/AlN multilayer coatings. 605.40 KB 70 downloads

High-temperature oxidation of CrN/AlN multilayer coatings. ...
Icon

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. 1.94 MB 67 downloads

Formation of a tetragonal Cu3Au alloy at gold/copper interfaces. ...
Icon

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer water. 2.35 MB 71 downloads

Evidence of multiple H+ ion desorption pathways with ESD of chemisorbed and multilayer...
Icon

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. 207.58 KB 72 downloads

Energetics of MCsn+ molecular ions emitted from Cs+ irradiated surfaces. ...
Icon

End point detection in ion beam milling of YB2 Cu3 07 thin films. 4.15 MB 67 downloads

End point detection in ion beam milling of YB2 Cu3 07 thin films. ...
Icon

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and indium. 252.94 KB 67 downloads

Dependence of scattered ion yield on the incident energy: Ne+ on pure gallium and...
Icon

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. 1.36 MB 67 downloads

Combustion Synthesis of Triangular and Multifunctional ZnON (x # 0.15) Materials. ...
Icon

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour deposition system. 1.03 MB 71 downloads

Characterization of TiO2 coatings prepared by a modified electric arc-physical vapour...