Overview

The spectrum below was measured from a uranium containing glass (under 1% wt.) using a 5keV oxygen primary ion beam and 500eV electron beam charge compensation. The 235U fraction is determined to be 0.55 ±0.02%; less than the 0.72% abundance expected from natural material.

QUANTIFICATION

Depth

SIMS depth profile data is collected as a function of sputter time which comprises the time taken for individual raster scanned frames and the number of frames in an analytical cycle. The most usual way to calibrate the depth scale is to measure the depth of the crater at the end of analysis (either using a surface profilometer or optical technique) and assume a constant sputter rate. In heterogeneous materials, different sputter rates can be applied for each component.

Concentration

The intensity scale is converted to concentration by comparison to a reference sample whose composition is well known. This can be a specially prepared material or a previously measured sample. It is even possible to use SNMS (built into many Hiden SIMS spectrometers) to calibrate in the high concentration region which can then be used to quantify low level impurities in SIMS.

Direct Comparison

In many cases it is unnecessary to fully quantify a measurement, instead the depth profiles can be directly compared to observe differences. This approach can work extremely well detecting changes from the norm in a production environment.

IMAGING

As the primary ion beam is scanned across the sample in a raster pattern, secondary ions are collected as a function of position allowing a mass resolved image to be produced at every cycle within a depth profile, so imaging is actually the primary method of data collection. The lateral resolution of an image depends on the primary ion beam spot size, the ultimate being when a SIMS detector is mounted on a focussed ion beam microscope (FIB) when resolutions of 10s of nm are possible.

Further Reading

Icon

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization... 330.25 KB 72 downloads

Surface Analysis under Ambient Conditions Using Plasma-Assisted Desorption/Ionization...
Icon

Surface Analysis by Secondary-Ion Mass Spectroscopy During Etching with Gas-Cluster Ion Beam 153.58 KB 85 downloads

Surface analysis by secondary-ion mass spectroscopy during etching with gas-cluster...
Icon

Sputter Depth Profiling by Secondary Ion Mass Spectrometry Coupled with Sample Current... 613.21 KB 78 downloads

Sputter depth profiling by secondary ion mass spectrometry coupled with sample current...
Icon

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS and... 109.76 KB 76 downloads

Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. 3. XPS...
Icon

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective 1.94 MB 76 downloads

Preferential Oxygen-Trapping in Metallic Multilayers: A SIMS Perspective. ...
Icon

Plasma Implanted Ultra Shallow Junction Boron Depth Profiles: Effect of Plasma Chemistry... 618.05 KB 79 downloads

Plasma implanted ultra shallow junction boron depth profiles: Effect of plasma chemistry...
Icon

Mass-Resolved Ion Scattering Spectrometry for Characterization of Samples with Historical... 200.29 KB 74 downloads

Mass-resolved ion scattering spectrometry for characterization of samples with historical...
Icon

Interfacial Diffusion in a Double Quantum Well Structure 1.94 MB 86 downloads

Interfacial diffusion in a double quantum well structure. ...
Icon

Interface-Dominated Growth of a Metastable Novel Alloy Phase 1.94 MB 74 downloads

Interface-dominated Growth of a Metastable Novel Alloy Phase. ...
Icon

Instantaneous Surface Work Function Dependence of MCs+n Molecular Ion Emission Under... 1.94 MB 71 downloads

Instantaneous surface work function dependence of MCs+n molecular ion emission under...