Select Page

FIB SIMS

Icon

Interfacial Nucleation Mechanisms in Reservoir-Free Na All Solid-State Batteries Using Ultrathin Interlayers and Low Stack Pressure 3.71 MB 0 downloads

Interfacial Nucleation Mechanisms in Reservoir-Free Na All Solid-State Batteries...
Icon

High-Throughput Combinatorial Analysis of the Spatiotemporal Dynamics of Nanoscale Lithium Metal Plating 11.56 MB 96 downloads

High-Throughput Combinatorial Analysis of the Spatiotemporal Dynamics of Nanoscale...
Icon

Combined Stabilizing of the Solid−Electrolyte Interphase with Suppression of Graphite Exfoliation via Additive-Solvent Optimization in Li-Ion Batteries 8.83 MB 70 downloads

Combined Stabilizing of the Solid−Electrolyte Interphase with Suppression of Graphite...
Icon

Differentially pumped quadrupole SIMS probe on FIB-based and two-beam microscopes 1.22 MB 97 downloads

Differentially pumped quadrupole SIMS probe on FIB-based and two-beam microscopes ...
Icon

Electrostatic Tuning of Ionic Charge in SiO2 Dielectric Thin Films 919.96 KB 89 downloads

Electrostatic Tuning of Ionic Charge in SiO2 Dielectric Thin Films ...
Icon

Experimental determination of Li diffusivity in LLZO using isotopic exchange and FIB-SIMS 1.27 MB 113 downloads